In copper-molybdenum circuits, the rougher concentrate is only half the battle. The hard part is what happens next: two sulphide minerals that floated together now have to be pulled apart, and the reagent that does most of that work is sodium hydrosulfide. Understanding how it behaves, how much to add, and what degrades it in storage separates a circuit that hits grade from one that circulates loads it cannot separate.
Why Sodium Hydrosulfide Depresses Copper
Sodium hydrosulfide, NaHS, is the acid salt of hydrogen sulphide and the most widely used depressant in copper-molybdenum separation. Its mechanism is not a simple pH effect. In solution it dissociates to supply hydrosulfide ions, which adsorb on copper sulphide surfaces and render them hydrophilic, while leaving molybdenite — a layered mineral with basal planes that are naturally hydrophobic — comparatively unaffected.
That selectivity is the whole point. A xanthate or a thionocarbamate will happily collect both chalcopyrite and molybdenite; NaHS selectively suppresses the copper minerals so that molybdenite can be floated away in the cleaner stages.
The practical consequence is a narrow operating window. Too little NaHS and copper reports to the molybdenum concentrate as a penalty element. Too much and molybdenite recovery falls, because excessive hydrosulfide begins to affect the molybdenite edges as well as the copper surfaces.

Grades, Assay and What You Are Actually Buying
Sodium hydrosulfide is traded in two main forms. The solid form is typically supplied as flakes or granules at around 70 percent NaHS, sometimes labelled by its total sulphide content rather than by the salt itself. The liquid form is a 30 to 40 percent solution delivered in IBC totes or road tankers.
The assay basis matters more than most buyers realise. A “70 percent” flake specification may refer to NaHS content, to total sulphur, or to sodium sulphide equivalent, and those three numbers are not interchangeable. Always ask which basis the certificate of analysis uses, and compare quotations on that basis rather than on the headline percentage.
Moisture, iron and sodium carbonate content are the impurities that most affect performance. Carbonate in particular builds up in closed process water circuits and can shift pulp chemistry in ways that show up as erratic cleaner performance weeks later.
Dosage and Circuit Practice
Typical NaHS addition in copper-molybdenum separation runs from two to ten kilograms per tonne of cleaner feed, staged across the cleaners rather than dosed at a single point. Staged addition is standard practice because the depressant is consumed by the minerals it adsorbs onto, and because the required concentration falls as the copper grade in the stream drops.
Three operating variables interact with NaHS and are worth monitoring together. Pulp pH controls the dissociation equilibrium and therefore the availability of hydrosulfide ions. Oxidation state matters because hydrosulfide is readily oxidised to thiosulphate and sulphate, both of which are far weaker depressants. And retention time matters because the adsorption is not instantaneous; short conditioner residence gives the appearance of under-dosing when the real problem is mixing.
Where NaHS is unavailable or where its hazards are unacceptable, alternatives include sodium sulphide, ammonium sulphide, thioglycolic acid and the various proprietary copper depressants. Each has a different cost and a different effect on downstream filtration and effluent, so a substitution should be tested rather than assumed equivalent.
Safety: The Part That Is Easy to Underestimate
Sodium hydrosulfide releases hydrogen sulphide in contact with acid, and H2S is lethal at concentrations well below the odour threshold’s reliable warning range. Olfactory fatigue sets in quickly, which means the smell cannot be trusted as a safety indicator.
Practical controls are non-negotiable: keep NaHS away from acidic streams and from acids used in cleaning, provide fixed H2S detection in the reagent area and in the thickener walkways, ventilate confined spaces before entry, and supply respiratory protection rated for H2S rather than dust masks. Liquid product splashes should be treated as caustic burns and rinsed immediately.
Liquid grades are easier to dose and meter accurately. Flake product is cheaper per tonne of active ingredient but requires dissolving equipment, generates dust and, if stored poorly, oxidises on the surface of the flakes before it ever reaches the circuit.
Storage, Degradation and Incoming Inspection
Both forms degrade with air and heat. Flakes should be kept sealed, dry and away from sunlight, and stock should rotate on a first-in-first-out basis; a drum left open in a humid store can lose a meaningful fraction of its activity within months. Liquid product should be stored in closed tanks with a nitrogen blanket where the value justifies it, and it must not be allowed to freeze.
Incoming inspection should include assay by iodometric titration, carbonate content, iron content and specific gravity for liquids. Retain a sealed sample per lot. If cleaner performance drifts, the depressant is one of the first suspects, and a retained sample turns a suspicion into evidence.
For the wider reagent context, the site’s guide to copper sulfate pentahydrate and sodium hydrosulfide in flotation covers how the activator and the depressant interact, and the flotation reagents complete guide sets out where regulators sit relative to collectors and frothers.
Conclusion
Sodium hydrosulfide earns its place in copper-molybdenum circuits because it does something no collector can: it separates two minerals that were floated together deliberately. Buying it well means comparing assay on a declared basis, checking carbonate and iron, specifying the physical form that suits your dissolving or dosing equipment, and treating the hydrogen sulphide hazard as a design requirement rather than a training slide.